Powder Metallurgical Tungsten Fiber-Reinforced Tungsten

Article Preview

Abstract:

The composite material tungsten fiber-reinforced tungsten (Wf/W) addresses the brittleness of tungsten by extrinsic toughening through introduction of energy dissipation mechanisms. These mechanisms allow the release of stress peaks and thus improve the materials resistance against crack growth. Wf/W samples produced via chemical vapor infiltration (CVI) indeed show higher toughness in mechanical tests than pure tungsten. By utilizing powder metallurgy (PM) one could benefit from available industrialized approaches for composite production and alloying routes. In this contribution the PM method of hot isostatic pressing (HIP) is used to produce Wf/W samples. A variety of measurements were conducted to verify the operation of the expected toughening mechanisms in HIP Wf/W composites. The interface debonding behavior was investigated in push-out tests. In addition, the mechanical properties of the matrix were investigated, in order to deepen the understanding of the complex interaction between the sample preparation and the resulting mechanical properties of the composite material. First HIP Wf/W single-fiber samples feature a compact matrix with densities of more than 99% of the theoretical density of tungsten. Scanning electron microscopy (SEM) analysis further demonstrates an intact interface with indentations of powder particles at the interface-matrix boundary. First push-out tests indicate that the interface was damaged by HIPing.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 825-826)

Pages:

125-133

Citation:

Online since:

July 2015

Export:

Price:

* - Corresponding Author

[1] R. Lässer et al., Structural materials for DEMO: The EU development, strategy, testing and modelling, Fusion Engineering and Design, 82 (2007) 511–520.

DOI: 10.1016/j.fusengdes.2007.06.031

Google Scholar

[2] H. Bolt et al., Plasma facing and high heat flux materials-needs for ITER and beyond, Journal of Nuclear Materials, 307-311 (2002) 43–52.

DOI: 10.1016/s0022-3115(02)01175-3

Google Scholar

[3] J. Reiser et al., Tungsten foil laminate for structural divertor applications – Basics and outlook, Journal of Nuclear Materials, 423 (2012) 1–8.

DOI: 10.1016/j.jnucmat.2012.01.010

Google Scholar

[4] J. Riesch et al., Enhanced toughness and stable crack propagation in a novel tungsten fibre-reinforced tungsten composite produced by chemical vapour infiltration, Phys. Scr. T159 (2014) 014031 (7pp).

DOI: 10.1088/0031-8949/2014/t159/014031

Google Scholar

[5] T. Hinoki et al., Silicon Carbide and Silicon Carbide Composites for Fusion Reactor Application, Materials Transactions, 54 (2013) 472-476.

DOI: 10.2320/matertrans.mg201206

Google Scholar

[6] J. Du, A feasibility study of tungsten-fiber-reinforced tungsten composites with engineered interfaces, Ph.D. Thesis, Technische Universität München, (2011).

Google Scholar

[7] J. Riesch et al., In-situ synchrotron tomography estimation of toughening effect by semi-ductile fibre reinforcement in a tungsten fibre-reinforced tungsten composite system, Acta Mat., 61 (2013) 7060–7071.

DOI: 10.1016/j.actamat.2013.07.035

Google Scholar

[8] M. -Y. He, J.W. Hutchinson, Crack deflection at an interface between dissimilar elastic materials, International Journal of Solids and Structures, 25 (1989) 1053-1067.

DOI: 10.1016/0020-7683(89)90021-8

Google Scholar

[9] B. Predel, Ta-W (Tantalum-Tungsten), Madelung, O. (ed. ), SpringerMaterials - The Landolt-Börnstein Database, DOI: 10. 1007/10551312_2793 (15. 02. 02).

Google Scholar

[10] ASTM Standard E407, 1999, Standard Practice for Microetching Metals and Alloys, ASTM International, West Conshohocken, PA, (1996).

Google Scholar

[11] ASTM Standard E112, 1996e3, Standard Test Methods for Determining Average Grain Size, ASTM International, West Conshohocken, PA, (1996).

Google Scholar

[12] W. Weibull, A Statistical Theory of the Strength of Materials, Ingeniors Vetenskaps Akademien, 151 (1939).

Google Scholar

[13] E. Lassner, W. -D. Schubert, Tungsten - Properties, Chemistry, Technology of the Element, Alloys and Chemical Compounds, Kluwer Academic/Plenum Publishers, (1999).

Google Scholar

[14] M.V. Aguirre et al., Mechanical Behavior of W-Y2O3 and W-Ti Alloys from 25 °C to 1000 °C, Metallurgical and Materials Transactions A, 40 (2009) 2283-2290.

DOI: 10.1007/s11661-009-9956-4

Google Scholar

[15] G. -M. Song, Y. -J. Wang, Y. Zhou, Thermomechanical properties of TiC particle-reinforced tungsten composites for high temperature applications, Int. J. of Refractory Metals and Hard Mat., 21 (2003) 1-12.

DOI: 10.1016/s0263-4368(02)00105-1

Google Scholar

[16] L. Redouani, S. Boudrahem, Hot isostatic pressing process simulation: application to metal powders, Canadian Journal of Physics, 90 (2012) 573-583.

DOI: 10.1139/p2012-057

Google Scholar

[17] N. Pan, Theoretical determination of the optimal fiber volume fraction and fiber-matrix property compatibility of short fiber composites, Polymer Composites, 14 (1993) 85-93.

DOI: 10.1002/pc.750140202

Google Scholar