Next Article in Journal
Enhanced Photocatalytic Activity of Nonuniformly Nitrogen-Doped Nb2O5 by Prolonging the Lifetime of Photogenerated Holes
Next Article in Special Issue
Mechanochemical Synthesis of Sustainable Ternary and Quaternary Nanostructured Cu2SnS3, Cu2ZnSnS4, and Cu2ZnSnSe4 Chalcogenides for Thermoelectric Applications
Previous Article in Journal
Zinc-Containing Sol–Gel Glass Nanoparticles to Deliver Therapeutic Ions
Previous Article in Special Issue
Enhanced Thermoelectric Properties of Te Doped Polycrystalline Sn0.94Pb0.01Se
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

A Bi2Te3-Filled Nickel Foam Film with Exceptional Flexibility and Thermoelectric Performance

1
College of Materials Science and Engineering, Nanjing Tech University, Nanjing 210009, China
2
Key Laboratory of Flexible Electronics of Zhejiang Province, Ningbo Institute of Northwestern Polytechnical University, Ningbo 315103, China
3
State Key Laboratory of High-Performance Ceramics and Superfine Microstructures, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, China
4
Radiation Technology Institute, Beijing Academy of Science and Technology, Beijing 100875, China
5
Key Laboratory of Beam Technology of Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, Beijing 100875, China
6
State Key Laboratory of New Ceramics and Fine Processing, School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China
7
Institute for Metallic Materials, Leibniz Institute for Solid State and Materials Research, 01069 Dresden, Germany
8
Micro-Nano Systems Centre, Tyndall National Institute, University College Cork, Dyke Parade, Lee Maltings, T12 R5CP Cork, Ireland
*
Author to whom correspondence should be addressed.
Nanomaterials 2022, 12(10), 1693; https://doi.org/10.3390/nano12101693
Submission received: 13 April 2022 / Revised: 27 April 2022 / Accepted: 9 May 2022 / Published: 16 May 2022

Abstract

:
The past decades have witnessed surging demand for wearable electronics, for which thermoelectrics (TEs) are considered a promising self-charging technology, as they are capable of converting skin heat into electricity directly. Bi2Te3 is the most-used TE material at room temperature, due to a high zT of ~1. However, it is different to integrate Bi2Te3 for wearable TEs owing to its intrinsic rigidity. Bi2Te3 could be flexible when made thin enough, but this implies a small electrical and thermal load, thus severely restricting the power output. Herein, we developed a Bi2Te3/nickel foam (NiFoam) composite film through solvothermal deposition of Bi2Te3 nanoplates into porous NiFoam. Due to the mesh structure and ductility of Ni Foam, the film, with a thickness of 160 μm, exhibited a high figure of merit for flexibility, 0.016, connoting higher output. Moreover, the film also revealed a high tensile strength of 12.7 ± 0.04 MPa and a maximum elongation rate of 28.8%. In addition, due to the film’s high electrical conductivity and enhanced Seebeck coefficient, an outstanding power factor of 850 μW m−1 K−2 was achieved, which is among the highest ever reported. A module fabricated with five such n-type legs integrated electrically in series and thermally in parallel showed an output power of 22.8 nW at a temperature gap of 30 K. This work offered a cost-effective avenue for making highly flexible TE films for power supply of wearable electronics by intercalating TE nanoplates into porous and meshed-structure materials.

1. Introduction

Flexible electronics (FEs) are an emerging electronic technology that integrates different material systems and different functional components on flexible substrates to form flexible devices and systems that can be stretched and bent. FEs subversively change the rigid physical form of traditional electronic devices and systems. So far, most FEs adopted traditional energy sources that require disassembly and cyclic charge/discharge, which bring in cost increases and inconvenience. For devices inserted into the human body, it is even hazardous. Thus, it is urgent to develop self-charging technology that could harvest energy from the ambient environment [1,2,3]. Flexible thermoelectrics (FTEs) could directly convert heat into electricity, and thus can be regarded as an alternative for powering FTEs that is long-lasting, reliable and safe [4]. The performance of thermoelectric (TE) materials can be evaluated via the TE figure of merit, zT = S2σT/κ, where S represents the Seebeck coefficient, σ is the electrical conductivity, κ is the thermal conductivity, T represents the absolute temperature of the environment, and the term S2σ is defined as the power factor, PF [5]. To date, Bi2Te3, with a rhombohedral structure and a band gap of 0.15 eV, is the most widely used TE material, since it has the best TE performance at room temperature among all materials. Because the Bi and Te atoms are bonded via covalent and ionic bonding, the Bi2Te3 lattice is rigid and poor in flexibility [6,7]. Making Bi2Te3 flexible remains a present issue.
Most solid materials, including intrinsically brittle ones such as ceramic and glasses, can become flexible when their thickness is small enough. Taking the inflexible and rigid crystalline silicon as an example, when its thickness is as low as 100 nm, it becomes flexible and can be utilized in wearable electronics [8]. Hence, it is important to take thickness into account when measuring flexibility. A common way to investigate the flexibility of a material is to conduct a bending test by attaching the material to a regular cylinder with a series of reduced bending curvatures until breakage [9]. Recently, Peng et al. [10] put forward a figure of merit for flexibility, fFOM, which could be expressed by the yield strain, ε, i.e., the degree of elastic deformation preceding plastic deformation at a given thickness. The maximum ε, considered as the relative degree of elongation on the inner/outer surface, can be simply figured out from the geometry: ε = h/2r, where h represents the thickness and r represents the critical bending curvature prior to breakage. Bi2Te3, as a rigid material, is nonexclusively flexible if sufficiently thin. For example, Shang et al. [11] physically sputtered a thin layer of Bi2Te3 with a thickness of 0.75 μm on polyimide, and Na et al. [12] electro-chemically deposited a thin layer of Bi2Te3 with a thickness of 2.6 μm on stainless-steel sheet. The Bi2Te3 layer was then peeled off by attaching to a piece of epoxy tape. Their fFOM values were lower than 4 × 10−5, which was ascribed to a small h but a large r. Polymers are intrinsically flexible, which can be used when forming composites with Bi2Te3. The Bi2Te3/PEDOT and Bi2Te3/PEDOT:PSS films synthesized by Wang [13] and Goo et al. [14], respectively, exhibited an increased fFOM of an order of 1 × 10−4. Bi2Te3/cellulose fibers and Bi2Te3/rGO film synthesized by Jin [15] and Ding et al. [16] revealed a further increased fFOM on the order of 4 × 10−3. Despite tremendous efforts to endow Bi2Te3-based thin films with a certain degree of flexibility, their thickness values are still small, implying restricted electrical and thermal loads, therefore limiting the maximal power output. Thus, attaining thicker and more flexible Bi2Te3 based film, meaning a larger fFOM, is a matter of urgency for real energy harvesting in wearable electronics.
Metal foams with porous and mesh structures have a great many properties that make them popular in a variety of applications, such as batteries and capacitors, among others [17,18]. Specifically, the capacity of metal foams to tolerate large strains (up to 60%) at a nearly constant stress can enable tremendous energy absorption without generating damaging peak stress, thus making them excellent candidates for energy absorption applications [17]. The energy from outer forces is also readily absorbed during bending deformation. Therefore, metal foams with porous and mesh structures are considered superior in terms of flexibility [19,20]. Nickel foam (NiFoam) is commercially available and cheap, and it has a high σ and an S with an absolute value second only to bismuth among all metals with negative S [21]. Open-cell NiFoam with a 3D thorough porous structure can allow Bi2Te3 nanoplates to enter, thus making a NiFoam/Bi2Te3 all-inorganic composite. It is expected to endow flexibility as well as to boost TE performance in the composite. In this work, we prepared a NiFoam/Bi2Te3 all-inorganic composite film using a solvothermal deposition method. The microstructures, performance and underlying mechanisms are discussed in detail.

2. Materials and Methods

Material synthesis and module integration: The material preparation and device synthesis process are shown in Figure 1. Firstly, a 20 mm × 20 mm segment of NiFoam was cut out and added into 3 M HCl aqueous solution under ultrasonication for 10 min. Then, the NiFoam was washed with deionized water and ethanol under ultrasonication for 10 min. This pretreatment could remove the oxide layer, as well as other contaminants such as grease. After that, the NiFoam was vacuum-dried at 303 K for 3 h. Secondly, 1 mM bismuth nitrate pentahydrate (Bi (NO3)3·5H2O, ≥99%, Aladdin, Los Angeles, USA), 1.5 mM sodium tellurite (Na2TeO3, ≥97%, Meryer, Shanghai, CHN), and 0.23 g polyvinylpyrrolidone (PVP, K30, Rhawn, Shanghai, CHN) were added into 30 mL ethylene glycol (EG, ≥99%, Yonghua Chemical, Suzhou, CHN) under stirring for 10 min. Then, 0.4 g sodium hydroxide (NaOH, ≥99%, Xilong Scientific, Shantou, CHN) was added under stirring until the precursor solution was clear. The precursor solution was then added along with the NiFoam into an autoclave, which was heated at 453 K for 12 h. The result was vacuum-dried at 333 K for 6 h to obtain the NiFoam/Bi2Te3 composite. In order to suppress the volatilization of Te in the high temperature film, the NiFoam/Bi2Te3 composite was pressed under 1 MPa and sealed together with Te powder in a quartz tube in vacuum. Then, the quartz tube was heated at 573 K for 90 min, and allowed to cool down to room temperature naturally. The obtained NiFoam/Bi2Te3 film was cut into legs with sizes of approximately 4 mm × 17 mm × 0.16 mm. Five such legs were integrated thermally in parallel and electrically in series with silver paste on the polyimide tape. In order to prevent possible oxidation, all the legs were sealed with polydimethylsiloxane (PDMS).
Microstructure characterization and performance measurement: The phases were characterized using X-ray diffractometry (XRD, Rigaku, Ultima IV) via CuKα radiation (1.5418 Å). GAGS software was used to perform Rietveld refinement, with an Rwp of approximately 5%, on the Bi2Te3 powder made by the solvothermal method and the annealed NiFoam/Bi2Te3 composite film. The microstructure of the film was characterized using field-emission scanning electron microscopy (FE-SEM, ZEISS, MERLIN Compact). A transmission electron microscope (TEM, Jeol, JEM 2010) was used to observe the microstructures of the nanoplates. XPS measurement was conducted on a Thermo Scientific ESCALAB 250Xi with a monochromated aluminum X-ray source (hv = 1486.6 eV), at a beam energy of 15 kV, a beam current of 10 mA and an incident angle of 58°, while an electron flood gun was used for charge compensation. The C peak at 284.6 eV was used to model other peaks and the Shirley algorithm was utilized to deduct base lines. The four-point probe system (LRIPER, LPPS100A) was used to test the electrical conductivity via the Van der Pauw method. The Seebeck coefficient was measured using a home-made system reported elsewhere [22]. Flexibility was characterized by attaching the film to the outer surfaces of glass tubes with different radii and evaluating the rate of change in resistivity. Tensile strength testing was performed on a sample with a size of 10 mm × 12 mm × 0.17 mm using a commercial multifunctional mechanical characterization device (EAST SUN, DR-5010A).

3. Results and Discussion

3.1. Phases and Microstructures

Figure 2a shows the XRD patterns of the NiFoam and the NiFoam/Bi2Te3 film before and after annealing. The XRD patterns of the pretreated NiFoam were consistent with the standard peaks of Ni (PDF#04-0850), and no other impurity phases were observed. It was considered that the possible oxide layers and grease on the surface of the NiFoam skeletons were removed during the pretreatment [23]. The raw materials Bi (NO3)3·5H2O and Na2TeO3 were used as Bi and Te sources, respectively. EG could coherently act as solvent and reducing agent, as the hydroxyl groups in EG are reducible under alkaline conditions with NaOH. Bi (NO3)3·5H2O and Na2TeO3 were first reduced to Bi and Te, respectively, and then Bi2Te3 was produced via atomic bonding. PVP could reduce the activities of Bi and Te for slow and stable generation of Bi2Te3 [24]. As shown in Figure 3a, the Bi2Te3 nanoplates revealed sharp edges and a regular hexagonal shape with an average diameter of approximately 600 nm, consistent with the TEM investigations. The crystal spacings of 0.219, 0.322 and 0.512 nm were assigned to the (0 1 0), (0 1 5) and (0 0 6) faces, respectively, of Bi2Te3 (Figure 3b).
The XRD pattern of the NiFoam/Bi2Te3 film prepared via the solvothermal method revealed both Ni peaks (PDF#04-0850) and Bi2Te3 peaks (PDF#15-0863), indicating that Bi2Te3 was in situ deposited into NiFoam (Figure 2a). After annealing, minor diffraction peaks of NiTe2 (PDF#08-0004) were also found as marked by the rhombi, indicating possible formation of a NiTe2 transition layer at the interface of Ni and Bi2Te3 during annealing [25]. This was confirmed by later XPS measurement. The relative intensity of the diffraction peak (1 0 1 0) at 37.8° before and after annealing was much greater than that of the Bi2Te3 standard card. This could be attributed to the pressing process, which possibly caused optimal orientation. As shown in the Rietveld refinement results in Figure 2b,c, the exact stoichiometry of the Bi2Te3 powder made using the solvothermal method was Bi1.76Te3.24. After depositing into NiFoam and subsequent annealing, the stoichiometry was refined to Bi1.9Te3.12, which was regarded as due to the formation of minor amounts of NiTe2 with a mass ratio of 3%. The weight fractions of Bi1.9Te3.12 and Ni were 72% and 25%, respectively.
Figure 3c shows a low-magnification image of the NiFoam where the three-dimensional porous structure is visible. The diameter of the through-holes was ~200 μm. The surface of the nickel skeleton was smooth after cleaning, with a skeleton width of ~50 μm (Figure 3d). The interior grain boundaries were clear after HCl corrosion. The Ni grain size was ~8 μm as indicated. As shown in Figure 4a,b, Bi2Te3 was successfully solvothermally deposited onto/into the NiFoam. The three-dimensional through-holes of the NiFoam were completely filled with Bi2Te3 nanoplates, and the Ni skeleton was also completely covered. The interfaces between the nanoplates were clear, implying that the interfacial bonding between them was weak. The black circle in the center of the nanoplates (Figure 4b) was reported to be due to Ostwald ripening at low reaction temperatures (≤463 K) [26]. After annealing, the film (Figure 4c,d) became relatively dense and smooth. Annealing improved the atomic diffusing and blurred the interfaces between the nanosheets, which was conducive to carrier transport [27]. This is corroborated via the improvement in the σ and mechanical stability of the films after annealing.
XPS spectra of the annealed NiFoam/Bi2Te3 film are shown in Figure 5. The survey scan in Figure 5a showed the major Bi, Te, and Ni peaks. There were some peaks of O and C. The presence of oxygen was mainly due to surface oxidation of Bi2Te3. The presence of carbon was due to surface hydrocarbon contaminants. In the Bi 4f curve (Figure 5b), two peaks at ≈158.7 and 163.9 eV were attributed to Bi 4f7/2 and Bi 4f5/2, respectively, revealing the existence of Bi2O3 and corresponding well to the reference values [28]. From the Te 3d curve (Figure 5c), the binding energies of Te 3d5/2 and Te 3d3/2 were 572.4 and 582.8 eV, respectively, which also corresponded well to the reference values, while the two peaks at 573 and 583.4 eV were attributed to NiTe2 [29]. The other two strong peaks were attributed to TeO2, confirming the surface oxidation of Bi2Te3. In the Ni 2p curve (Figure 5d), the peaks at 873.70 and 855.5 eV were attributed to Ni(OH)2, according to the NIST XPS database [30], which might be due to a surface reaction between Ni and NaOH.

3.2. Mechanical Properties

Both XRD patterns and XPS spectra revealed the formation of the NiTe2 phase during annealing. The formed NiTe2 was sandwiched between Ni and Bi2Te3, forming a core–shell structure (Ni/NiTe2/Bi2Te3-x) (Figure 6b). This enhanced the mechanical bonding between Ni and Bi2Te3. Therefore, the mechanical stability and durability could be improved. Since nickel and Bi2Te3 were regarded as simply combined via the Van der Waals force before annealing (Figure 6a), Bi2Te3 could be easily stripped off from the nickel frame during ultrasonication as can be seen in Figure 6c. This did not occur for the film after annealing (Figure 6d).
Figure 7a is a photograph of a composite film undergoing flexibility testing. When the bending radius was reduced from 10 mm to 5 mm (Figure 7b), the decrease in σ was less than 10% compared to the flat state. The film was then subjected to 25–100 bending cycles at a bending radius of 5 mm. The decrease in σ was still less than 10% (Figure 7c). This indicates excellent mechanical flexibility of the NiFoam/Bi2Te3. Figure 7d lists the value of the fFOM from recently published Bi2Te3-based alloys and composites, and it can be seen that our NiFoam/Bi2Te3 film had a fFOM value of more than three times higher than others, which shows that the film has excellent flexibility.
As is known, wearable electronics are sometimes under tensile stress. It is thus significant to characterize the tensile strength of the TE films for wearable usage. Figure 8 shows the tensile–elongation curves of NiFoam and the annealed NiFoam/Bi2Te3 film. The unit shape of the NiFoam could be regarded as a regular hexagon (Figure 8, Stage I). When the hexagonal NiFoam began to stretch, it first deformed from a regular hexagon to a rectangle, and the theoretical elongation according to geometry at this time was ~17%. After that, there was considered to be an elastic deformation period and a yield stage, which were not obvious in the curve. Then, a plastic stage continued until the maximum stress, 6.5 ± 0.02 MPa. The elongation at this point was 21% (Figure 8, Stage II). After that, the instability fracture stage came, showing necking deformation until breakage. At this point, the maximum elongation was 27.5% (Figure 8, Stage III). For the NiFoam/Bi2Te3 film, the maximum tensile strength was 12.7 ± 0.04 MPa, which was twice that of NiFoam, due to the strengthening effect of the bonded Bi2Te3. As shown in Figure 8, during stage I to stage II, the Bi2Te3 was first compressed and stretched concurrently with the initial geometry deformation of NiFoam. Bi2Te3 has a rigid intrinsic nature; it is weaker in tension than it is in compression. The tensile strength is often at least one order of magnitude lower than the compressive strength for many brittle materials [31]. It was considered that horizontal cracks would form first in Bi2Te3 and then extend to the skeleton of the NiFoam. The maximum elongation, 28.8%, did not change much due to the rigid nature of Bi2Te3.
As shown in Table 1, compared with the TE films reported, the as-prepared NiFoam/Bi2Te3 film exhibited the best elongation overall. Its tensile stress of 12.7 ± 0.04 MPa was higher than that of CNT/PDMS, PPBH/CNT/PUBI, or PEDOT/SWCNT/BC, and comparable to that of DMSO/PEDOT:PSS, PEDOT:PSS/Rubber, or PVDF/Ni, which were based on intrinsic flexible organics. Moreover, as the NiFoam/Bi2Te3 film showed the best PF, which was ~2 orders of magnitude higher than the above materials, it can be concluded that the NiFoam/Bi2Te3 film displayed the best comprehensive performance for flexible energy harvesting.

3.3. Thermoelectric Properties and Power Generation of Module

As shown in Figure 9, after solvothermal deposition of Bi2Te3 nanoplates onto/into the three-dimensional networked NiFoam, σ was slightly decreased, from 1066.1 S cm−1 to 1000.9 S cm−1. This was due to the much lower intrinsic σ in Bi2Te3 compared to NiFoam, as the mass fraction of Bi2Te3 reached 58.2%. However, filling Bi2Te3 into the through-holes of NiFoam could provide additional carrier transport paths, which might increase mobility. This would help maintain the σ without much degradation. After annealing, the σ was increased from 1000.9 S cm−1 to over 1107.8 S cm−1. Because annealing could reduce defects in the Bi2Te3, decrease the boundary density, and bridge the nickel skeleton and Bi2Te3 by generating transition phases, it was possible for it to increase the mobility. The absolute value of S of the NiFoam/Bi2Te3 film increased from 17.7 μV K−1 for NiFoam to 22.2 μV K−1, due to the weighting effect as the intrinsic S of Bi2Te3 was higher than NiFoam. After annealing, the absolute value of S was further increased to 27.7 μV K−1, which was due to the reduction in carrier concentration caused by NiTe2 formation and evaporation of trace Te. The PF of the composite film before annealing reached 493 μW m−1 K−2, which was 1.5 times that of pure NiFoam. After annealing, the PF further increased to 850 μW m−1 K−2, 2.5 times that of pure NiFoam. The geometry of the Bi2Te3 filling the foam pores could be approximated as being spherical, and therefore the thermal conductivity of the as-prepared NiFoam/Bi2Te3 film could be estimated to be 1.7 W m−1 K−1 based on the Woodside and Messmer model [38], κ c = κ m p × κ s 1 p , where κ c , κ m and κ s are the thermal conductivity of the composite, Bi2Te3, and nickel, respectively, and p is the original porosity. The corresponding TE figure of merit, zT, was thus calculated to be 0.15, which is lower than the magnetically sputtered Bi2Te3-based films [39]. Nevertheless, it had a much larger thickness (160 μm), two orders of magnitude higher, than the sputtered film, implying a much higher tolerance of electrical and thermal load and thus a higher power output.
In order to demonstrate power generation by a TE module based on the as-prepared NiFoam/Bi2Te3 composite films, five strips with a size of~ 4 mm × 17 mm × 0.16 mm were cut out and connected electrically in series using silver paste on a piece of polyimide film (Figure 10a). As shown in Figure 10b, when the TE module was held with one end on the wrist with the other end exposed to air, the maximum open circuit voltage was 0.32 mV. When one end of the TE module was attached to arm skin, while a piece of cloth was placed between the other end and the skin for increasing thermal resistance (to develop a thermal gradient), a maximum open circuit voltage was of 0.29 mV was achieved (Figure 10c). Therefore, the TE module could be used to collect skin heat and convert it into power at ambient temperature. In order to further demonstrate power generation by the TE module under different temperature differences, one end of the TE module was attached to a heating plate and the other end was exposed to air. By adjusting the power of the heating plate, different temperature differences, ΔT, could be established (Figure 10d). The open circuit voltages of the TE module were 0.61 mV, 1.86 mV, 3.12 mV, and 3.75 mV at temperature differences of 5 K, 15 K, 25 K, and 30 K, respectively. These measured values were consistent with the theoretical values evaluated via V0 = ΔT × |S| × N, where |S| is the absolute S and N is the total number of thermoelectric legs. To demonstrate the power output of the TE module under various temperature differences, an external resistor was connected to form a power measurement circuit based on voltammetry. The power output P of the module could thus be expressed as:
P = E 2 ( R e x R i n ) 2 R e x + 4 R i n  
where Rex is the resistance of the external resistor, Rin is the total internal resistance of the module and the ammeter. For a fixed ΔT, the output voltage (E) is a constant, while the P could reach maximum at Rex = Rin. Figure 10e,f shows the curves of power and voltage output vs. the current of the circuit at ∆T = 10 K, 20 K, and 30 K, respectively. At ∆T = 10 K, Rex = 150 Ω and Pmax = 1.95 nW, with the voltage and the current being 1.09 mV and 6.87 mA, respectively. At ∆T = 20 K, Rex = 140 Ω and Pmax = 10.28 nW, with the voltage and current being 2.38 mV and 11.24 mA, respectively. At ∆T = 30 K, Rex = 137 Ω and Pmax = 22.76 nW, with the voltage and current being 3.62 mV and 24.92 mA, respectively. The TE module could provide an output power of several tens of nW under a small temperature difference. Moreover, it is flexible and bendable. Thus, our NiFoam/Bi2Te3 based thermoelectric generator has the potential to be used for a variety of miniature sensors and wearable devices, such as for powering temperature and humidity sensors, blood pressure sensors, heartbeat sensors, bracelets, etc.

4. Conclusions

In conclusion, we prepared a NiFoam/Bi2Te3 composite film that exhibited a high PF of 850 μW m−1 K−2 and excellent mechanical flexibility as well as high tensile strength. Its figure of merit for flexibility could reach 0.016, and its tensile strength and breaking elongation were 12.7 ± 0.04 MPa and 28.8%, respectively. This composite material was fabricated by solvothermal deposition of Bi2Te3 nanoplates into/onto porous NiFoam followed by annealing. The generation of a transition layer of NiTe2 during annealing could enhance bonding between the NiFoam skeleton and the Bi2Te3, thereby boosting its mechanical stability. A thermoelectric (TE) module was assembled with five legs with dimensions of ~4 mm × 17 mm × 0.16 mm. The output voltage of the TE module was 3.75 mV and the output power was 22.8 nW at a temperature difference of 30 K. Due to the low cost of commercial NiFoam as well as the simplicity of synthesis, the Bi2Te3/NiFoam film demonstrated great potential for powering wearable electronics by harvesting energy from human skin. This work provides a cost-effective method for making exceptionally flexible and high-performance TE films for energy harvesting by intercalating TE nanoplates into a porous meshed nickel structure that is intrinsically flexible.

Author Contributions

Conceptualization, P.-a.Z.; methodology, T.S., M.C. and Q.Z.; software, T.S., P.-a.Z.; validation, Z.M., J.Z. and Q.H.; formal analysis, P.-a.Z., T.S., K.M.R., Z.W. and Q.S.; investigation, Y.O., H.W. and J.L.; resources, Z.L.; data curation, Z.M.; writing—original draft preparation, T.S.; writing—review and editing, P.-a.Z.; visualization, T.S.; supervision, P.-a.Z.; project administration, P.-a.Z.; funding acquisition, P.-a.Z. and Q.S. All authors have read and agreed to the published version of the manuscript.

Funding

This research was supported by the Natural Science Foundation of Jiangsu Province (no. BK20211264), the Natural Science Fund for Colleges and Universities in Jiangsu Province (no. 21KJB430023), the Priority Academic Program Development of Jiangsu Higher Education Institutions (PAPD), Natural Science Foundation of China (no. 51702183), the Opening Project of State Key Laboratory of High-Performance Ceramics and Superfine Microstructure (no. SKL202004SIC), the Innovation and Entrepreneurship Program of Jiangsu Province (no. JSSCBS20210418), and research funds from the Department of Science and Technology of Shaanxi Province (No. D5140200091/2020GXLH-Z-009; D5140200101/2020GXLH-Z-019), the Ningbo Natural Science Foundation (202003N4370), the European Union’s Horizon 2020-funded project under grant agreement no. 825114 (SmartVista), Science Foundation Ireland (SFI) and the European Regional Development Fund under Grant Number 15/IA/3160, 12/RC/2276 and 13/RC/2077.

Institutional Review Board Statement

Not applicable.

Data Availability Statement

Not applicable.

Acknowledgments

The authors acknowledge G. Jeffery Snyder from Northwestern University, USA, and Chunlei Wan from Tsinghua University, China for fruitful discussions.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Yoo, J.Y.; Yang, J.S.; Chung, M.K.; Kim, S.H.; Yoon, J.B. A review of geometric and structural design for reliable flexible electronics. J. Micromech. Microeng. 2021, 31, 074001. [Google Scholar] [CrossRef]
  2. Kwak, S.; Kang, J.; Nam, I.; Yi, J. Free-form and deformable energy storage as a forerunner to next-generation smart electronics. Micromachines 2020, 11, 347. [Google Scholar] [CrossRef] [PubMed] [Green Version]
  3. Leung, S.F.; Ho, K.T.; Kung, P.K.; Hsiao, V.K.S.; Alshareef, H.N.; Wang, Z.L.; He, J.H. A self-powered and flexible organometallic halide perovskite photodetector with very high detectivity. Adv. Mater. 2018, 30, 1704611. [Google Scholar] [CrossRef] [PubMed]
  4. He, W.; Zhang, G.; Zhang, X.; Ji, J.; Li, G.; Zhao, X. Recent development and application of thermoelectric generator and cooler. Appl. Energ. 2015, 143, 1–25. [Google Scholar] [CrossRef]
  5. Soleimani, Z.; Zoras, S.; Ceranic, B.; Cui, Y.; Shahzad, S. A comprehensive review on the output voltage/power of wearable thermoelectric generators concerning their geometry and thermoelectric materials. Nano Energy 2021, 89, 106325. [Google Scholar] [CrossRef]
  6. Manzano, C.V.; Abad, B.; Munoz Rojo, M.; Koh, Y.R.; Hodson, S.L.; Lopez Martinez, A.M.; Xu, X.; Shakouri, A.; Sands, T.D.; Borca-Tasciuc, T.; et al. Anisotropic effects on the thermoelectric properties of highly oriented electrodeposited Bi2Te3 films. Sci. Rep. 2016, 6, 19129. [Google Scholar] [CrossRef] [Green Version]
  7. Fu, J.; Huang, J.; Bernard, F. Electronic structure, elastic and optical properties of Bi2Te3/Sb2Te3 thermoelectric composites in the periodic-superlattice thin films. Compos. Commun. 2021, 28, 100917. [Google Scholar] [CrossRef]
  8. Rogers, J.A.; Someya, T.; Huang, Y. Materials and mechanics for stretchable electronics. Science 2010, 327, 1603–1607. [Google Scholar] [CrossRef] [Green Version]
  9. Wan, C.G.; Dang, X.; Itoh, F.; Wang, T.; Sasaki, Y.; Kondo, H.; Koga, M.; Yabuki, K.; Snyder, K.; Yang, G.J.; et al. Flexible n-type thermoelectric materials by organic intercalation of layered transition metal dichalcogenide TiS2. Nat. Mater. 2015, 14, 622–627. [Google Scholar] [CrossRef]
  10. Peng, J.; Snyder, G.J. A figure of merit for flexibility. Science 2019, 366, 690. [Google Scholar] [CrossRef]
  11. Shang, H.D.; Deng, C.; Li, Y.; Gao, T.; Xiao, Z.; Gu, L.; Singh, H.; Ren, D.J.; Ding, Z. Bi0.5Sb1.5Te3-based films for flexible thermoelectric devices. J. Mater. Chem. 2020, 8, 4552–4561. [Google Scholar] [CrossRef]
  12. Na, J.; Kim, Y.; Park, T.; Park, C.; Kim, E. Preparation of bismuth telluride films with high thermoelectric power factor. ACS Appl. Mater. Interfaces 2016, 8, 32392–32400. [Google Scholar] [CrossRef] [PubMed]
  13. Wang, L.Z.; Liu, Z.; Wang, Y.; Fang, B.; Qiu, L.; Zhang, J.; Wang, K. Exceptional thermoelectric properties of flexible organic−inorganic hybrids with monodispersed and periodic nanophase. Nat. Commun. 2018, 9, 3817. [Google Scholar] [CrossRef] [PubMed]
  14. Goo, G.; Anoop, G.; Unithrattil, S.; Kim, W.S.; Lee, H.J.; Kim, H.B.; Jung, M.H.; Park, J.; Ko, H.C.; Jo, J.Y. Proton-irradiation effects on the thermoelectric properties of flexible Bi2Te3/PEDOT:PSS composite films. Adv. Electron. Mater. 2019, 5, 1800786. [Google Scholar] [CrossRef]
  15. Jin, Q.S.; Zhao, W.; Qiao, Y.; Qiu, J.; Sun, J.; Lei, C.; Tai, H.; Jiang, K. Cellulose fiber-based hierarchical porous bismuth telluride for high-performance flexible and tailorable thermoelectrics. ACS Appl. Mater. Interfaces 2018, 10, 1743–1751. [Google Scholar] [CrossRef] [PubMed]
  16. Ding, D.F.; Sun, F.M.; Xia, F.; Tang, Z.Y. A high-performance and flexible thermoelectric generator based on the solution-processed composites of reduced graphene oxide nanosheets and bismuth telluride nanoplates. Nanoscale Adv. 2020, 2, 3244–3251. [Google Scholar] [CrossRef]
  17. Edison, T.N.J.I.; Atchudan, R.; Karthik, N.; Ganesh, K.; Xiong, D.; Lee, Y.R. A novel binder-free electro-synthesis of hierarchical nickel sulfide nanostructures on nickel foam as a battery-type electrode for hybrid-capacitors. Fuel 2020, 276, 118077. [Google Scholar] [CrossRef]
  18. Wang, J.; Zhao, Y.; Zhang, D.; Li, Y.; Song, S.; Ke, Y. Emerging NiCo2O4 electrode materials assembled by nanosheets for high performance hybrid capacitor with high specific capacitance. J. Nanoelectron. Optoelectron. 2020, 15, 498–503. [Google Scholar] [CrossRef]
  19. Olurin, O. Strength and ductility of as-plated and sintered CVD nickel foams. Compos. Sci. Technol. 2003, 63, 2317–2329. [Google Scholar] [CrossRef]
  20. Lee, K.; Lewandowski, J.J. Effects of microstructural characteristics on mechanical properties of open-cell nickel foams. Mater. Sci. Technol.-Lond. 2013, 21, 1355–1358. [Google Scholar] [CrossRef]
  21. Fujita, S.; Ho, H.C.; Okamura, Y. Quantum theory of the Seebeck coefficient in metals. Int. J. Mod. Phys. B 2000, 14, 2231–2240. [Google Scholar] [CrossRef]
  22. Zong, P.A.; Zhang, P.; Yin, S.; Huang, Y.; Wang, Y.; Wan, C. Fabrication and characterization of a hybrid Bi2Se3/organic superlattice for thermoelectric energy conversion. Adv. Electron. Mater. 2019, 5, 842. [Google Scholar] [CrossRef]
  23. Hao, S.; Liu, J.W.; Cao, Q.; Zhao, Y.H.; Zhao, X.B.; Pei, K.; Zhang, J.; Chen, G.Y.; Che, R.C. In-situ electrochemical pretreatment of hierarchical Ni3S2-based electrocatalyst towards promoted hydrogen evolution reaction with low overpotential. J. Colloid Interface Sci. 2020, 559, 282–290. [Google Scholar] [CrossRef] [PubMed]
  24. He, H.; Huang, D.; Zhang, X.; Li, G. Characterization of hexagonal Bi2Te3 nanosheets prepared by solvothermal method. Solid State Commun. 2012, 152, 810–815. [Google Scholar] [CrossRef]
  25. Yaprintsev, M.; Vasil’ev, A.; Ivanov, O.; Zhezhu, M.; Yaprintseva, E.; Novikov, V. Forming the locally-gradient Ni@NiTe2 domains from initial Ni inclusions embedded into thermoelectric Bi2Te3 matrix. Mater. Lett. 2021, 290, 129451. [Google Scholar] [CrossRef]
  26. Yuichi, H.; Koji, T.; Masayuki, T. Growth of single-crystalline Bi2Te3 hexagonal nanoplates with and without single nanopores during temperature-controlled solvothermal synthesis. Sci. Rep. 2019, 9, 10790. [Google Scholar] [CrossRef] [Green Version]
  27. Hosokawa, Y.; Wada, K.; Tanaka, M.; Tomita, K.; Takashiri, M. Thermal annealing effect on structural and thermoelectric properties of hexagonal Bi2Te3 nanoplate thin films by drop-casting technique. Jpn. J. Appl. Phys. 2018, 57, 02CC02. [Google Scholar] [CrossRef]
  28. Chen, X.; Feng, L.; Yu, P.; Liu, C.; Lan, J.; Lin, Y.H.; Yang, X. Flexible thermoelectric films based on Bi2Te3 nanosheets and carbon nanotube network with high n-type performance. ACS Appl. Mater. Interfaces 2021, 13, 5451–5459. [Google Scholar] [CrossRef]
  29. Chia, X.; Sofer, Z.; Luxa, J.; Pumera, M. Unconventionally layered CoTe2 and NiTe2 as electrocatalysts for hydrogen evolution. Chemistry 2017, 23, 11719–11726. [Google Scholar] [CrossRef]
  30. Naumkin, A.V.; Kraut-Vass, A.; Gaarenstroom, S.W.; Powell, C.J. NIST X-ray Photoelectron Spectroscopy Database; Version 4.1; National Institute of Standards and Technology: Gaithersburg, MD, USA, 2012. Available online: http://srdata.nist.gov/xps/ (accessed on 1 April 2022).
  31. Gerda, R.; Peter, R. Mechanical properties of skutterudites. Sci. Adv. Mater. 2011, 3, 517–538. [Google Scholar] [CrossRef]
  32. Kang, Y.H.; Bae, E.J.; Lee, M.H.; Han, M.; Kim, B.J.; Cho, S.Y. Highly flexible and durable thermoelectric power generator using CNT/PDMS foam by rapid solvent evaporation. Small 2022, 18, 2106108. [Google Scholar] [CrossRef] [PubMed]
  33. Kee, S.; Haque, M.A.; Corzo, D.; Alshareef, H.N.; Baran, D. Self-healing and stretchable 3D-printed organic thermoelectrics. Adv. Funct. Mater. 2019, 29, 1905426. [Google Scholar] [CrossRef]
  34. Yang, Y.; Zhao, G.; Cheng, X.; Deng, H.; Fu, Q. Stretchable and healable conductive elastomer based on PEDOT:PSS/natural rubber for self-powered temperature and strain sensing. ACS Appl. Mater. Interfaces 2021, 13, 14599–14611. [Google Scholar] [CrossRef] [PubMed]
  35. Hu, S.; Zeng, S.; Li, X.; Jiang, J.; Yang, W.; Chen, Y.; Li, M.; Zheng, J. Flexible and high performance of n-type thermoelectric PVDF composite film induced by nickel nanowires. Mater. Des. 2020, 188, 108496. [Google Scholar] [CrossRef]
  36. Xiao, C.; Xue, Y.; Liu, M.; Xu, X.; Wu, X.; Wang, Z.; Xu, Y.; Chen, G. Polymer composites with lychee-like core covered by segregated conducting and flexible networks: Unique morphology, high flexibility, stretchability and thermoelectric performance. Compos. Sci. Technol. 2018, 161, 16–21. [Google Scholar] [CrossRef]
  37. Jia, F.; Wu, R.; Liu, C.; Lan, J.; Lin, Y.H.; Yang, X. High thermoelectric and flexible PEDOT/SWCNT/BC nanoporous films derived from aerogels. ACS Sustain. Chem. Eng. 2019, 7, 12591–12600. [Google Scholar] [CrossRef]
  38. Zhou, L.; Yang, L. A method to calculate the effective thermal conductivity of spherical particle-laden composite. IOP Conf. Ser. Mater. Sci. Eng. 2019, 493, 012049. [Google Scholar] [CrossRef]
  39. Jin, Q.; Jiang, S.; Zhao, Y.; Wang, D.; Qiu, J.; Tang, D.M.; Tan, J.; Sun, D.M.; Hou, P.X.; Chen, X.Q.; et al. Flexible layer-structured Bi2Te3 thermoelectric on a carbon nanotube scaffold. Nat. Mater. 2019, 18, 62–68. [Google Scholar] [CrossRef]
Figure 1. Schematic diagram of the synthesis of NiFoam/Bi2Te3 composite film and module fabrication.
Figure 1. Schematic diagram of the synthesis of NiFoam/Bi2Te3 composite film and module fabrication.
Nanomaterials 12 01693 g001
Figure 2. (a) XRD patterns of NiFoam and NiFoam/Bi2Te3 composite film before and after annealing. Rietveld refinement results of (b) solvothermally prepared Bi2Te3 powder and (c) annealed NiFoam/Bi2Te3 composite.
Figure 2. (a) XRD patterns of NiFoam and NiFoam/Bi2Te3 composite film before and after annealing. Rietveld refinement results of (b) solvothermally prepared Bi2Te3 powder and (c) annealed NiFoam/Bi2Te3 composite.
Nanomaterials 12 01693 g002
Figure 3. (a) SEM and (b) TEM images of the solvothermally deposited Bi2Te3 nanoplates; (c) low- and (d) high-magnification SEM images of NiFoam.
Figure 3. (a) SEM and (b) TEM images of the solvothermally deposited Bi2Te3 nanoplates; (c) low- and (d) high-magnification SEM images of NiFoam.
Nanomaterials 12 01693 g003
Figure 4. SEM images of NiFoam/Bi2Te3 composite film before (a,b) and after annealing (c,d) with low to high magnifications.
Figure 4. SEM images of NiFoam/Bi2Te3 composite film before (a,b) and after annealing (c,d) with low to high magnifications.
Nanomaterials 12 01693 g004
Figure 5. X-ray photoelectron spectra of (a) survey scan, (b) Bi 4f region, (c) Te 3d region, and (d) Ni 2p region for the annealed NiFoam/Bi2Te3 film.
Figure 5. X-ray photoelectron spectra of (a) survey scan, (b) Bi 4f region, (c) Te 3d region, and (d) Ni 2p region for the annealed NiFoam/Bi2Te3 film.
Nanomaterials 12 01693 g005
Figure 6. Schematic diagrams of the changes in the NiFoam/Bi2Te3 interface (a) before and (b) after annealing, and photos showing possible stripping under sonication for NiFoam/Bi2Te3 film (c) before (collapse) and (d) after annealing (stable).
Figure 6. Schematic diagrams of the changes in the NiFoam/Bi2Te3 interface (a) before and (b) after annealing, and photos showing possible stripping under sonication for NiFoam/Bi2Te3 film (c) before (collapse) and (d) after annealing (stable).
Nanomaterials 12 01693 g006
Figure 7. (a) Photograph illustrating resistivity test via the four-probe method where the NiFoam/Bi2Te3 film was bent and attached to a glass tube; (b) ratio of resistivity at bending state (R) to flat state (Ro) at different bending radii (r); (c) R/Ro under a series of bending cycles at r = 5 mm; (d) the figure of merit for flexibility (fFOM) of Bi2Te3-based TE films reported and in this work.
Figure 7. (a) Photograph illustrating resistivity test via the four-probe method where the NiFoam/Bi2Te3 film was bent and attached to a glass tube; (b) ratio of resistivity at bending state (R) to flat state (Ro) at different bending radii (r); (c) R/Ro under a series of bending cycles at r = 5 mm; (d) the figure of merit for flexibility (fFOM) of Bi2Te3-based TE films reported and in this work.
Nanomaterials 12 01693 g007
Figure 8. Curves of tensile strength vs. elongation of NiFoam and NiFoam/Bi2Te3 film; the inset is the schematic diagram of tensile processes of NiFoam and the annealed NiFoam/Bi2Te3 composite film.
Figure 8. Curves of tensile strength vs. elongation of NiFoam and NiFoam/Bi2Te3 film; the inset is the schematic diagram of tensile processes of NiFoam and the annealed NiFoam/Bi2Te3 composite film.
Nanomaterials 12 01693 g008
Figure 9. Electrical conductivity (σ), Seebeck coefficient (S) and power factor (PF) of NiFoam and NiFoam/Bi2Te3 film before and after annealing.
Figure 9. Electrical conductivity (σ), Seebeck coefficient (S) and power factor (PF) of NiFoam and NiFoam/Bi2Te3 film before and after annealing.
Nanomaterials 12 01693 g009
Figure 10. (a) Photograph of the assembled TE module; (b) voltage output when the TE was held against the wrist or (c) attached onto the arm with one end exposed to the air; (d) output voltage of the TE module at different temperature differences; (e) output voltage and (f) output power of the TE module under temperature differences of 10 K, 20 K and 30 K.
Figure 10. (a) Photograph of the assembled TE module; (b) voltage output when the TE was held against the wrist or (c) attached onto the arm with one end exposed to the air; (d) output voltage of the TE module at different temperature differences; (e) output voltage and (f) output power of the TE module under temperature differences of 10 K, 20 K and 30 K.
Nanomaterials 12 01693 g010
Table 1. Tensile strengths and power factors of TE films.
Table 1. Tensile strengths and power factors of TE films.
CompositionTensile Strength
(MPa)
Elongation
(%)
Power Factor
(μW m−1 K−2)
Ref.
CNT/PDMS Foam0.7820.62.9[32]
DMSO/PEDOT:PSS38.976.6108.9[33]
PEDOT:PSS/Rubber20.124.019.1[34]
PVDF/Ni nanowires25.3 9.024.3[35]
PPBH/CNT/PUBI6.113.86.3[36]
PEDOT/SWCNT/BC1.62.112.0[37]
Ni Foam/Bi2Te312.7 ± 0.0428.8850.0This work
Notes: CNT: carbon nanotubes, PDMS: polydimethylsiloxane, DMSO: Dimethyl sulfoxide, PEDOT:PSS: Poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate), PVDF: poly(1,1-difluoroethylene), PPBH: polymer particles bearing many small bumps and crosslinkable hydroxyl groups on their surfaces, PUBI: water dispersible polyurethane with blocked terminal isocyanate groups [36], PAA: Polyacrylic acid, CA: Cellulose acetate, SWCNT: single-wall carbon nanotube, BC: Bacterial cellulose.
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Shi, T.; Chen, M.; Liu, Z.; Song, Q.; Ou, Y.; Wang, H.; Liang, J.; Zhang, Q.; Mao, Z.; Wang, Z.; et al. A Bi2Te3-Filled Nickel Foam Film with Exceptional Flexibility and Thermoelectric Performance. Nanomaterials 2022, 12, 1693. https://doi.org/10.3390/nano12101693

AMA Style

Shi T, Chen M, Liu Z, Song Q, Ou Y, Wang H, Liang J, Zhang Q, Mao Z, Wang Z, et al. A Bi2Te3-Filled Nickel Foam Film with Exceptional Flexibility and Thermoelectric Performance. Nanomaterials. 2022; 12(10):1693. https://doi.org/10.3390/nano12101693

Chicago/Turabian Style

Shi, Taifeng, Mengran Chen, Zhenguo Liu, Qingfeng Song, Yixiang Ou, Haoqi Wang, Jia Liang, Qihao Zhang, Zhendong Mao, Zhiwen Wang, and et al. 2022. "A Bi2Te3-Filled Nickel Foam Film with Exceptional Flexibility and Thermoelectric Performance" Nanomaterials 12, no. 10: 1693. https://doi.org/10.3390/nano12101693

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop