Home > Journals > Minerva Dental and Oral Science > Past Issues > Minerva Stomatologica 2020 June;69(3) > Minerva Stomatologica 2020 June;69(3):153-8

CURRENT ISSUE
 

JOURNAL TOOLS

Publishing options
eTOC
To subscribe
Submit an article
Recommend to your librarian
 

ARTICLE TOOLS

Publication history
Reprints
Permissions
Cite this article as
Share

 

ORIGINAL ARTICLE   

Minerva Stomatologica 2020 June;69(3):153-8

DOI: 10.23736/S0026-4970.19.04291-2

Copyright © 2019 EDIZIONI MINERVA MEDICA

language: English

Evaluation of bond strength of dual resin cements to CAD/CAM-created lithium disilicate ceramic

Felipe SCZEPANSKI 1, Cláudia R. BRUNNQUELL 2, Sandrine B. BERGER 3, Eloisa A. PALOCO 3, Murilo B. LOPES 3, Amauri C. DRUMOND 3, Alejandra H. GONZÁLEZ 3, Ricardo D. GUIRALDO 3

1 Department of Dentistry, State University of North Paraná (UENP), Jacarezinho, Brazil; 2 Department of Physiotherapy, State University of North Paraná (UENP), Jacarezinho, Brazil; 3 Department of Restorative Dentistry, University of North Paraná (UNOPAR), Londrina, Brazil



BACKGROUND: The objective was to examine the microshear bond strength values of different dual resin cements to computer-aided design (CAD)/computer-aided manufacturing (CAM)-created ceramics containing lithium disilicate, which underwent different surface treatments.
METHODS: Two dual resin cements (RelyX ARC and RelyX Ultimate) and three surface treatments of lithium disilicate ceramic blocks (Ceramic Primer (CP; containing silane) plus Adper Scotchbond Multipurpose (ASM) adhesive; CP plus Single Bond Universal (SBU) adhesive; and SBU adhesive alone) were tested. The SBU adhesive includes silane in its formulation. Each sample underwent a microshear test and bond strength values were subjected to analysis of variance (ANOVA) followed by Tukey’s test (α=0.05). Fracture patterns were also observed with light microscopy.
RESULTS: RelyX ARC treated with CP+ASM or CP+SBU presented resistance values that were significantly higher than the same treatments for RelyX Ultimate. Conversely, for the blocks treated with SBU alone, the mean resistance value for RelyX Ultimate was higher than that of RelyX ARC. Regarding the different types of treatment for each resin, the mean resistance value of RelyX ARC treated with CP+ASM was significantly highest, followed by treatment with CP+SBU and SBU treatment alone. Meanwhile, RelyX Ultimate treated with CP+ASM or CP+SBU presented resistance values that were significantly higher than SBU treatment alone. In all of the groups, an adhesive fracture pattern was predominantly observed.
CONCLUSIONS: The present results indicate that silanization is important for ASM and SBU adhesives to be effective.


KEY WORDS: Ceramics; Shear strength; Cementation