Biron M.: “Thermoplastics and Thermoplastic Composites”, Second edition, Elsevier, Oxford 2013, p. 31.
[2] Zhang Y.C., Xu G.L., Liang Y. et al.: Thermochimica Acta 2016, 643, 33.
Crossref
[3] Pack S.: “Flame Retardants, Engineering Materials” (Eds. Visakh P., Arao Y.), Springer, Cham 2015, p. 115.
Crossref
[4] Yang S., Wang J., Huo S. et al.: Polymer Degradation and Stability 2015, 115, 63. ht tp: //dx.doi .org/10.1016/ j .polymdegradstab. 2015.02.016
[5] Hu W., Zhan J., Hong N. et al.: Polymers for Advanced Technologies 2014, 25, 631.
Crossref
[6] Perret B., Schartel B., Stöß K. et al.: European Polymer Journal 2011, 47, 1081.
Crossref
[7] Zhang W., Li X., Yang R.: Polymer Degradation and Stability 2011, 96, 2167. ht tp: //dx.doi .org/10.1016/ j .polymdegradstab. 2011.09.016
[8] Ebdon J.R., Price D., Hunt B.J. et al.: Polymer Degradation and Stability 2000, 69, 267.
Crossref
[9] Bourbigot S., Duquesne S.: Journal of Materials Chemistry 2007, 17, 2283.
Crossref
[10] Krala G., Ubowska A., Kowalczyk K.: Polymer Engineering & Science 2014, 54, 1030.
Crossref
[11] Chen X., Gu A., Liang G. et al.: Polymer Degradation and Stability 2012, 97, 698. ht tp: //dx.doi .org/10.1016/ j .polymdegradstab.2012.02.013
[12] Feldman D., Barbalata A.: “Synthetic Polymers. Technology, Properties, Applications”, Chapman & Hall, London 1996, p. 58.
[13] Gilman J.W., Kashiwagi T.: “Environmentally Safe Fire Retardants for Polymeric Materials. Part 1. Silica Gel: Potassium Carbonate Additive”, Symposium materials, 41st International SAMPE Symposium, March 24–28, 1996, p. 708.
Google Scholar