Abstract
In the experiment was monitored the influence of thermal-technical properties by binder amount. As binder was used organic based glue 4,4´MDI (Conipur 360). At the same time was verified possible dilution of binder with water. The binder was diluted in amounts of 5, 10, 15, 20, 25 and 30%. However, in the case of 25 and 30% has not been achieved complete dilution. Recycled plastic EVA (ethyl vinyl acetate) was used as filler.