Microstructure features of failure and mechanical properties of ultra-fine grained Ti–6AL–4V ELI alloy at 300–77 K

  • Published:
International Journal of Mechanics and Materials in Design Aims and scope Submit manuscript

Abstract

Experimental investigation of mechanical characteristics and failure regularities of the ultra-fine grained Ti–6Al–4V ELI alloy, produced by equal channel angular pressing (ECAP), have been carried out under the uniaxial tension at 300 and 77 K. These characteristics have been compared for the different structural states of the Ti–6Al–4V ELI alloy, distinguished by the average grain size and by the morphology of α and β phases. It has been established that the combination of the heat treatment, ECAP, and the extrusion of the Ti–6Al–4V ELI alloy leads to a considerable increase of the alloy’s strength in comparison with the initial state (54% at 300 K and 78% at 77 K) with preserving the reasonable values of the ductility (3–4% elongation to the neck beginning and 5–10% to the failure). For all investigated structural states of the Ti–6Al–4V ELI alloy only ductile failure was observed at 300 and 77 K. The fracture surface consists of regions failed under normal and shear stresses. In shear failure regions of fracture surface only elongated dimples were present.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Fig. 1
Fig. 2
Fig. 3
Fig. 4
Fig. 5
Fig. 6
Fig. 7
Fig. 8

Similar content being viewed by others

Abbreviations

ECAP:

Equal channel angular pressing

UFG:

Ultra-fine grained

OM:

Optical micrograph

TEM:

Transmission electron microscopy

References

  • Kim, S.M., Kim, J., Ko, Y.G., Lee, C.S., Shin, D.H.: Microstructure Development and segment formation during ECA pressing of Ti–6Al–4V alloy. Scripta Mater. 50, 927–930 (2004)

    Article  Google Scholar 

  • Liao, S., Duffy J.: Adiabatic shear bands in a Ti–6Al–4V titanium alloy. J. Mech. Phys. Solids. 46, 2201–2231 (1998)

    Article  Google Scholar 

  • Margolin, H., Mahajan Y.: Void formation, void growth and tensile fracture in Ti–6Al–4V. Metall. Trans. A 9A, 781–791 (1978)

    Google Scholar 

  • Semenova, I.P., Saitova, L.R., Raab, G.I., Valiev, R.Z.: Effect of severe plastic deformation on mechanical properties and structure of Ti alloys. In: Proceedings of the 8th ESAFORM Conference on Material Forming, vol. 2, pp. 661–664. Cluj-Napoca, Romania (2005a)

  • Semenova, I.P., Saitova, L.R., Raab, G.I., Korshunov, A.I., Zhu, Y.T., Lowe, T.C., Valiev, R.Z.: Microstructural features and mechanical properties of the Ti–6Al–4V ELI alloy processed by severe plastic deformation. In: Proceedings of the International conference “Nanomaterials by severe plastic deformation”, pp. 757–762. Fukuoka, Japan, September 22–26, 2005 (2005b)

  • Stolyarov, V.V., Zhu, Y.T., Alexandrov, I.V., Lowe, T.C., Valiev, R.Z.: Refinement and properties of pure Ti processed by warm ECAP and cold rolling. Mater. Sci. Eng. A343, 43–50 (2003)

    Google Scholar 

  • Tabachnikova, E., Bengus, V., Natsik, V., Csach, K., Miskuf, J., Stolyarov, V., Valiev, R.: Deformation and failure of Ti–6Al–4V nanostructured alloy at 300–4.2 K. In: Zhu, Y.T., Varyukhin, V. (eds.) Nanostructured Materials by High-Pressure Severe Plastic Deformation, pp. 259–263. Springer, Dordrecht (2006)

    Chapter  Google Scholar 

  • Weiss, I., Semiatin, S.L.: Thermomechanical processing of alpha titanium alloys-an overview. Mater. Sci. Eng. A263, 243–256 (1999)

    Google Scholar 

Download references

Acknowledgements

This work has been carried out with a partial financial support by the project No. 38/05-H of the NASU complex program “Nanosystems, nanomaterials and nanotechnologies”. The authors are indebted to M. I. Bidylo for assistance in experiments.

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Elena D. Tabachnikova.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Tabachnikova, E.D., Bengus, V.Z., Podolskiy, A.V. et al. Microstructure features of failure and mechanical properties of ultra-fine grained Ti–6AL–4V ELI alloy at 300–77 K. Int J Mech Mater Des 4, 189–195 (2008). https://doi.org/10.1007/s10999-007-9036-0

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s10999-007-9036-0