Abstract
The solubility product of aluminum nitride in 3 pct silicon iron was determined experimentally from 1273 to 1473 K with results described by the equation
whereT is in kelvins and concentrations are in weight percent. In the experiments the equilibrium distribution of nitrogen between purified gamma iron (fcc) and 3 pct silicon alpha iron (bcc) was determined between 1273 and 1523 K.
Similar content being viewed by others
References
H. A. Wriedt and H. Hu:Met. Trans. A., 1976, vol. 7A, p. 711.
T. Masumoto, M. Naka and Y. Imai:Nippon Kinzoku Gakkaishi, 1970, vol. 34, p. 195.
E. T. Turkdogan and S. Ignatowicz:J. Iron Steel Inst., 1957, vol. 185, p. 200.
S. Taguchi and A. Sakakura:Acta Metall., 1966, vol. 14, p. 405.
L. S. Darken, R. P. Smith, and E. W. Filer:Trans. AIME, 1951, vol. 191, p. 1174.
H. A. Wriedt and O. D. Gonzalez:Trans. TMS-AIME, 1961, vol. 221, p. 532.
N. S. Corney and E. T. Turkdogan:J. Iron Steel Inst., 1955, vol. 180, p. 344.
M. L. Pearce:Trans. TMS-AIME, 1963, vol. 227, p. 1393.
P. Grieveson and E. T. Turkdogan:Trans. TMS-AIME, 1964, vol. 230, p. 1604.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Wriedt, H.A. Solubility product of aluminum nitride in 3 percent silicon iron. Metall Trans A 11, 1731–1736 (1980). https://doi.org/10.1007/BF02660528
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF02660528