This paper describes the preparation and properties of (Na0.5Bi0.5)1 − x A x TiO3 (A = Sr, Cd) lead-free ferroelectric ceramics. The (0.63–0.66)Na0.5Bi0.5TiO3 · (0.37–0.34)Sr0.7Bi0.2TiO3 ceramics are shown to have the best dielectric and piezoelectric properties: tanδ = 0.013–0.009, ɛRT = 1200–1500, d 31 = (370–400) × 10−12 C/N, and k ρ = 0.4–0.58. The cadmium-containing ceramics offer low dielectric losses and high dielectric permittivity at room temperature.
Similar content being viewed by others
References
Rodel, J., Wook, J., Klaus, T., et al., Perspective on the Development of Lead-Free Piezoceramics, J. Am. Ceram. Soc., 2009, vol. 92, pp. 1153–1177.
Aksel, E. and Jones, J.L., Advances in Lead-Free Piezoelectric Materials for Sensors and Actuators, Sensors, 2010, vol. 10, pp. 1935–1954.
Shannon, R.D., Revised Effective Ionic Radii and Systematic Studies of Interatomic Distances in Halides and Chalcogenides, Acta Crystallogr., Sect. A: Cryst. Phys., Diffr., Theor. Gen. Crystallogr., 1976, vol. 32, no. 5, pp. 751–767.
Wei-Chih Lee, Tsao Chi-Yuen, Liang-Kuo, and Yu-Chun Wu, Chemical Composition and Tolerance Factor at the Morphotropic Phase Boundary in (Bi0.5Na0.5)TiO3-Based Piezoelectric Ceramics, J. Eur. Ceram. Soc., 2009, vol. 29, no. 8, pp. 1443–1448.
Isupov, V.A., Ion Ordering and Ferroelectricity in Pb(B′0.5B″0.5) O3 Perovskites, Phys. Solid State, 2007, vol. 49, pp. 505–509.
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Russian Text © A.I. Akimov, G.K. Savchuk, A.K. Letko, 2011, published in Neorganicheskie Materialy, 2011, Vol. 47, No. 11, pp. 1346–1351.
Rights and permissions
About this article
Cite this article
Akimov, A.I., Savchuk, G.K. & Letko, A.K. Preparation and properties of ceramics based on (Na0.5Bi0.5)1 − x A x TiO3 (A = Sr, Cd) solid solutions. Inorg Mater 47, 1227–1232 (2011). https://doi.org/10.1134/S0020168511100013
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1134/S0020168511100013