Summary
-
1.
The relationship between the density and pressure, during the compression at room temperature of steel chips and iron powder, can be expressed by thesame equation γ = γco−0.43 K0/α · e−2.3αP.
-
2.
The same relationship for hot compression of steel chips is expressed by the equation γ = a · P +γ arb·
Similar content being viewed by others
Literature cited
S. I. Stepanov, Poroshkovaya metallurgiya, No. 5, 81 (1964).
G. A. Vinogradov and I. D. Radomysel'skii, Pressing and Rolling of Cermets [in Russian], Mashgiz (1963).
N. F. Kunin and B. D. Yurchenko, Poroshkovaya metallurgiya, No. 6, 3 (1963).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Stepanov, S.I. Some laws on the hot and cold compression of steel chips. Powder Metall Met Ceram 5, 99–101 (1966). https://doi.org/10.1007/BF00775554
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF00775554